ASTM Testing Standards

...

Expand
titleReported during the test:
  • Force versus crosshead displacement, force versus deflection data continuously, or at frequent intervals (around 2-3 recordings per second, with a target minimum of 100 recorded data points)

  • If there are any initial failures, record force, displacement and mode of damage where the failure occurs. 

  • Record mode, area and location of each failure. 

  • Use the failure identification codes, shown in the figure below.

  • Record the max force, failure force, head displacement and the deflection at the moment of ultimate failure. 

  • For ultimate failure modes, record the mode, area and location of ultimate failure for each material. 

  • Calculations:

    • For 3-Point Mid-Span Loading:

    • For 4-Point, Quarter-point loading:

    • For 4-Point (Third Point) Loading:

ASTM D3039_Standard Test Methods for Tensile Properties

...

Expand
titleProcedure:

  • Apply the adhesive in accordance with the adhesive suppliers recommendations. 

  • Adhesive Cure—Cure the adhesive at room temperature or elevated temperature using prescribed conditions determined by the adhesive supplier.

  • Condition the test specimens

  • Place specimens in UTM

  • Wait for failure

Variable

Quantity

Grip Separation

75mm

load rate

13mm/min

...