Material

Curing Process

Lap Shear Strength (MPa)

Aluminum (acid etched)

Cured for 2 hrs at @ 65 deg C

13.7

Steel (grit blasted)

Cured for 12 hours @ 65 deg C

30

Aluminum (acid etched & abraded), 0.1 to 0.2 mm gap

33

Aluminum (anodised)

14

Stainless steel

23

Polycarbonate

6.9

Nylon

2.3

Wood (Fir)

11.3

...