greyish- warm/soft white
attach of fabric (grey or it could be coloured)
according to Google fabric materials are:
Fabric: 33% nylon, 67% polyester
Hydrophobic and antimicrobial coating
Polycarbonate (hard plastic)
could add colour to fibreglass / or colour it afterward
if we are sticking with google home aesthetic, just need to make sure that it looks like the white colour they use
maybe the first 3 colours? white colour with a tint of grey/beige
this colour was used in google store #F8F8F8 in hex
What to include:
top of each cover must be marked with letters at least 10mm high with
“Caution: Chemical Hazard”
“High Voltage”
type of the battery (ex. Li-ion)
any other standard hazard marking specific to the type of battery as well
indicates contravention of the regulation
provisions (like regulations I believe) to seal battery/enclosure - be made by the team
to prevent unauthorized actions
Style:
MS fonts, colours
thinking of small rectangle / square seal
How to make 3D printing less 3D printed looking
key point is: how can we smoothen out the surface?
Method
How-to
Pros
Cons
Sources
Sanding
will need different seams
after sanding, spray filler and spray paint can make the parts to look not like 3D printed
able adjust how smooth we want the surface to be
can be accurate in a way since we are sanding the parts that we want
could make a mistake of sanding to much
if it is a large part, time consuming to sand the whole part
https://www.youtube.com/watch?time_continue=258&v=NLoB52nPuao&feature=emb_logo
https://www.youtube.com/watch?v=0vgynnYzo08
Using Acetone
pour small amount of acetone into the glass that has paper towel in it
put the model inside the glass, and put a small fan in it so that the air moves
displace water around so acetone doesn’t leak
acetone will melt the 3D model
take it out, and dry the 3D model
acetone does its job to smooth our the surface
takes only about an hour
must be printed with ABS (Acrylonitrile Butadiene Styrene)
which gives toxic chemical when heated
shrinks when it is cold
not suitable
when doing this, could be dangerous since it is flammable
details can be gone
https://www.youtube.com/watch?v=6xFUNFG-UKE
https://www.youtube.com/watch?v=rn4edNztaPU
Using Spray paint / Spray Fast drying polyurethane
spray paint (more than usual) then spray a layer fast drying polyurethane, fan it
do this multiple times
no need to sand the 3D model
the details might be gone
Shorter Layer height
set the layer height as a low number
no need to do an extra step of smoothing out the surface
time consuming
longer the time, easier for the machine to get jam and stuck
3M Marine Adhesive Sealant 4200 Fast Cure
a way to attach fabric on boats
contact cement
extremely strong chemical, might be to extreme
industrial velcro
any fabric glue
could even make a small gap on the cover and insert the corners of the fabric